13
$\begingroup$

Since I have a 3D printer, I worked primarily with printing ABS. I tried multiple methods for adhesion (various soluble glues, ABS juice) but always had the most success with hairspray on clean borosilicate glass, as long as I print with a bed temperature above 75 °C and inside an enclosure.

So I wonder, if it is known, why and based on which chemicals the hairspray method works so well?

$\endgroup$
  • 2
    $\begingroup$ Hairspray is not ABS specific - it is just in need of a very strong bond. $\endgroup$ – Trish Oct 16 '19 at 8:39
12
$\begingroup$

First of all, not all hairsprays work. The chemicals in hairspray that causes the bonding is "VA/Crotonates Copolymer", it is also called "vinyl acetate/crotonic acid copolymer". Most commonly known as PVA, which is also a filament used as water soluble support material. This is a synthetic polymer created from monomers.

When heated to a certain temperature this ingredient becomes sticky, this makes the filament stick to the plate. It is the double bonded Oxygen molecule that makes this happen. This is not only present in chemicals you put onto the bed, but also the chemistry of certain bed materials. Quoting our own Ryan Carlyle from this thread, A replacement for Aquanet Hair Spray?? Wolfbite by Airwolf:

Most of the popular build surfaces have very similar underlying chemistry. That's because they all rely on diffusion welding for adhesion. The molecular chains at the interface slightly dissolve into each other.

Gluestick active ingredient - http://en.wikipedia.org/wiki/Polyvinylpyrrolidone

enter image description here

Aquanet and liquid PVA glue active ingredient - http://en.wikipedia.org/wiki/Polyvinyl_acetate

enter image description here

If you're familiar with organic chemistry, what you see here is an identical polyvinyl backbone chain, and functional groups that both have a ketone/ester double-bonded oxygen adjacent to a space-filling component. (The space-filling component probably decreases adhesion so the print can be released.) And guess what? Permanent build plate surfaces rely on the same underlying chemistry:

Lexan also has exposed double-bonded oxygen on a polymer backbone: http://en.wikipedia.org/wiki/Polycarbonate

enter image description here

Kapton also has exposed double-bonded oxygen on a polymer backbone: http://en.wikipedia.org/wiki/Kapton

enter image description here

Acrylic also has exposed double-bonded oxygen on a polymer backbone: http://en.wikipedia.org/wiki/Poly(methyl_methacrylate)

enter image description here

PET also has exposed double-bonded oxygen on a polymer backbone: http://en.wikipedia.org/wiki/Polyethylene_terephthalate

enter image description here

Now, if you look at some common solvents for filaments, what do you often see? Double-bonded oxygen on small molecules. Here's ethyl acetate (dissolves PLA) and acetone (dissolves ABS):

enter image description hereenter image description here

These molecules are still diffusing into the filament polymer, but they're so small and mobile that they are able to completely liquefy and dissolve the plastic.

Isn't chemistry great?

$\endgroup$
  • 3
    $\begingroup$ Isn't PVA what's in common white school glue (Elmer's in the US)? $\endgroup$ – T.J.L. Oct 16 '19 at 14:27
  • 1
    $\begingroup$ @T.J.L.Yes, white wood glue and white school glue also contain PVA (polyvinyl acetate), it is a PVA dispersion in water. $\endgroup$ – 0scar Oct 16 '19 at 14:31
  • 3
    $\begingroup$ To think, I glue my hair together every morning ... #OhTheJoy ;-) $\endgroup$ – Pᴀᴜʟsᴛᴇʀ2 Oct 16 '19 at 18:01
  • $\begingroup$ @Pᴀᴜʟsᴛᴇʀ2, send picture of hair :) $\endgroup$ – user77232 Oct 17 '19 at 17:57
  • 3
    $\begingroup$ @user77232 - Here you go. $\endgroup$ – Pᴀᴜʟsᴛᴇʀ2 Oct 17 '19 at 18:12

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.