5
$\begingroup$

In analogy to: What glues for bonding printed PLA to injection-molded plastic?, what are the best glues to use for PETG?

I mostly print in PETG and have occasional failed prints which I usually reprint. But what if I'd like to repair a print e.g. a split between layers or a part broken off?

Knowing that PETG is more "greasy" than PLA, what typical glues can you use to create a good bond; this question excludes using heat to (re-)bond.

$\endgroup$
2
$\begingroup$

From forum

Bison plastic - works great for me, only it's not "quick dry" but it's very strong, not brittle, holds PETG and PLA very strongly. Buy paint stripper that is/contains methylene chloride (dichloromethane). It will solvent weld both PLA and PETG.

Or see other forum which recommends Eastman-910 (original brand of cyanoacrylate) or any equivalent, polyurethane glue, or even epoxy.

$\endgroup$
2
$\begingroup$

A strong epoxy like BSI 5-15 min works great for me. I use it to bond high power rocket fin halves printed from PETG:

enter image description here

$\endgroup$
0
1
$\begingroup$

If Carl's answer that cyanoacrylate glue works is accurate, I would suggest Loctite 420 or equivalent. It's diluted with solvents sufficiently to behave as a liquid rather than a gel, and in my experience on PLA it not only bonds the joint, but wicks between the extrusions and bonds walls/layers together much more strongly and waterproofs the part. As long as it bonds to PETG it should do the same for PETG.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.