Recently, my Ender 3 printer is giving these bad quality prints as shown in the image below. Something in common in all these bad prints is that they only fail in a particular section. The print looks good on the rest of the parts. I'm having trouble on how to find people with similar problems as I don't know what type of failure this is called. I would really appreciate any suggestions on how to fix this or if anyone experienced the same issue and managed to solve this.

enter image description here

enter image description here

enter image description here

$\endgroup$
4
  • 1
    $\begingroup$ Hi, welcome to 3DPrinting.SE! Are your belts tight? $\endgroup$ – 0scar Dec 1 '20 at 23:05
  • $\begingroup$ Looks underextruded from bad temperature to me $\endgroup$ – Trish Dec 2 '20 at 13:39
  • $\begingroup$ I agree with @Trish, very similar to an under extrusion issue I had with my Ender 3. In my particular case it was because the nozzle was clogged. $\endgroup$ – Dr. Mantis Tobbogan Dec 6 '20 at 1:38
  • $\begingroup$ I'm with @0scar, looks like a belt is loose. $\endgroup$ – Galaxy Dec 7 '20 at 13:04