I am printing ABS on an Ender 3 printer at a temperature of 240 °C on the nozzle and 110 °C on the bed. I am getting the following result:

enter image description here

Is there any way I can fix this?

$\endgroup$
1
  • $\begingroup$ Have you tried lower bed temperatures? $\endgroup$
    – Perry Webb
    May 17 '21 at 14:05
1
$\begingroup$

I think that your bed is too hot because the bubbling is only on the bottom layer, if it was through out the entire print, I would say that it is your nozzle temp and you should do a temp tower, but because that isn't the case try lowering your bed temp

$\endgroup$