0
$\begingroup$

enter image description here

Can anyone help explain what might be wrong to do this? I am printing a bunch of the same item.

$\endgroup$
5
  • $\begingroup$ Which were the first and last items printed? $\endgroup$
    – Perry Webb
    May 23, 2022 at 15:50
  • 1
    $\begingroup$ My initial thought was insufficient bed adhesion, but it looks like you have a PEI sheet which I am not very familiar with its adhesion capabilities. $\endgroup$
    – agarza
    May 23, 2022 at 16:15
  • $\begingroup$ @PerryWebb It started in the middle and I think went clockwise layer by layer, but I didn't want everything. $\endgroup$
    – Doug
    May 23, 2022 at 16:38
  • $\begingroup$ @agarza Typically, prints are stuck pretty well to the bed, but come to think of it I haven't had anything print to the left side of the board much and it all seems to be that side. Maybe this is a slight level issue causing bed adhesion problems. I'll play around with it. Thanks! $\endgroup$
    – Doug
    May 23, 2022 at 16:39
  • 1
    $\begingroup$ @Doug I recall seeing an unboxing video recently where the reviewer was having a slight issue with the PEI sheet. After washing it with dish soap, the sheet was gripping the prints again. Just a thought. $\endgroup$
    – agarza
    May 23, 2022 at 21:26

0