Cura 2.4 reports that the (printer-dependant) G-Code mode prevents the "Flow" (extrusion rate adjustment percentage) setting from being available. Why? I am using an Ultimaker 2+. Is a firmware update required?

I know the "Flow" can by dynamically adjusted on the 3D printer (either in materials or while printing).

I am asking because I have small holes (1 mm) that seem to slice fine but get filled so the extrusion probably is not that optimally tuned. I suspected reducing the material rate would improve this but changing it on the printer (97%) did not yield noticable results and below that it looked worse.

$\endgroup$
2
$\begingroup$

For the Ultimaker 2 flow is typically handled on the printer.

You could make a feature request at github to let Flow be enabled for Ultimaker 2 printers.

As for your problem: that sounds more like a dimensional accuracy problem to me. I suggest setting Horizontal Expansion to -0.15mm.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.