I apologize if this is in the wrong section, but it seems relevant.
I am an absolute noob at 3D printing, but recently my need for a specific, small part intersected with access to a 3D printer at work (Zortrax M200), so I figured now was a good opportunity to get into printing.
I am designing a clamp for smaller can capacitors that will hold them upright from a mounting surface. I would like the capacitors to snap into the clamp, but I am struggling to find information on how wide the opening to the clamp should be. It clearly needs to be smaller than the diameter of the clamp, but I'm not sure how much smaller it can be without snapping the clamp arms.
Is there a rule of thumb or general guideline for this type of geometry? I am using Z-ULTRAT, which is some proprietary filament made by Zortrax. It seems to be similar to ABS in terms of strength properties, but stiffer.
I don't have an image at the moment, but I can provide one tomorrow when I have access to the part files. The best analog I can think of is a LEGO figure's hands.
Thanks.
Edit: Per requests for additional information:
I am not sure what is considered a "thin" wall; currently, the clamp walls are 2mm thick at the thinnest point (where the push-in opening is).
I would like the walls to be just flexible enough to allow the cap to be seated without breaking - it is more critical that the cap is not loose in the socket.
The clamp is not going to be subject to repeated stress cycles - by the time the cap needs replacing, it's likely I'll need to print a new clamp as well.
With my estimations for cooling, I do not expect the clamp to see temperatures above 100C.
Edit 2:
Based on the link in the comments below, I came up with the following design:
The little nubbins in the back fit into the "neck" at the bottom of the capacitor to provide some positive lock. 220 degrees of surround with 4mm thick arms - I think this should work.