I would like to know what are the best settings for Taulman 618 Nylon filament? In particular, the print head and print bed temperatures.

$\endgroup$
2
  • $\begingroup$ Best for what? These things depend on a lot of variables (like your printer, print speed, layer height, etc...). $\endgroup$ Commented May 3, 2017 at 8:41
  • $\begingroup$ Hi Cynthia, and welcome to Stack Exchange - 3D Printing. Please could you expand your answer, with more detail, as Tom has requested in his comment. The more information that you provide the more likely it is that someone will be able to provide you with an accurate answer. Also, take a look at How do I ask a good question?. Thanks. $\endgroup$
    – Greenonline
    Commented May 3, 2017 at 13:44

1 Answer 1

1
$\begingroup$

240°C, lots of cooling.

See Material Specification Print Sheet - Taulmann 618 Nylon.

$\endgroup$
1
  • $\begingroup$ Note: sometimes, for Nylon, I tape some fine sandpaper, grit up, and print on that. This gives more texture for the Nylon to adhere to. $\endgroup$