4
$\begingroup$

I'm searching for a truly clear DLP resin which can polymerize between 400nm and 405nm.

I found the unpigmented from FunToDo, but it seems to be yellow-clear:

enter image description here

I'm trying to achieve something similar to this:

enter image description here

Is there any resin out there which costs likely the same (about 50€/liter) which will give results like this?

$\endgroup$
2
$\begingroup$

Formlabs sells a completely clear resin that they've even made simple lenses from, but it's about $150 for a liter. I have no idea how well it would work with your DLP setup. Looks amazing in the pictures though.

MatterHackers sells PhotoCentric UV Firm Clear for $90 for a liter as well. It's not quite as easy finding pictures of this stuff, but from what it looks like, it's still pretty decent. Assuming you've got a UV DLP

Disclaimer, the PhotoCentric stuff says it's a UV resin (10nm to 400nm IIRC) and I have not the slightest clue what Formlabs designs their resin for, so YMMV.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.