For some reason, the bottom few layers printed on my Ender 3 are distorted. Used the benchy from http://www.3dbenchy.com/ and Cura 3.6.0, sliced with default settings for Ender 3 on the draft preset. The material is Hatchbox PLA. I think the bed is leveled pretty well, but there might be some adjustments I could make.Warping on the bottom layers

$\endgroup$
2
  • $\begingroup$ Please post an image of the bottom, usually this effect is caused by a too large of a nozzle to bed distance, this question, and the printed result, looks very much like asked here. $\endgroup$
    – 0scar
    Feb 6 '19 at 7:02
  • $\begingroup$ It may not be a duplicate as the dup's OP determined that the solution didn't actually resolve the issue. $\endgroup$ Feb 6 '19 at 18:43