3D printer filament will not load after running the printer out of filament

We wanted to test the post process properties of PVA but did not want to print anything. We unloaded the ABS that was in the printer and then started loading some PVA. After the PVA was loaded we ...
31
votes
2answers
2k views

How to recycle filament material from printed parts?

Is it possible to re-use ABS or PLA filament material from printed parts? If so, what is the techniques to reform it?
9
votes
4answers
890 views

Why is my print displacing along the y-axis by 2-3 cm?

I am encountering a problem with this ID3 printer using ABS -- at some point during the print the print head displaces on the y-axis by 2-3 centimeters. I cannot pinpoint how or why it is doing this. ...
23
votes
5answers
4k views

Does filament have to be stored in an airtight environment?

For standard ABS and PLA filament, most distributors recommend storing the filament in an airtight bag. Does not doing this actually make print quality worse? I have left mine in the open for a year ...
28
votes
11answers
23k views

Why do the corners of my ABS object lift off the bed?

I print ABS on a LulzBot Taz 5 and frequently have issues with the corners of objects lifting off the bed. My extruder is at 230 °C and the bed is at 90 °C for the first layer and 100 °...
20
votes
4answers
8k views

Would 3d-printed objects outgas in vacuum?

I want to fabricate a sample holder and shadow masks to use in vacuum chambers. The type of printing material is not important to me PLA/ABS/PC-ABS/nylon). I'm worried that 3d printed objects (FDM) ...
8
votes
4answers
12k views

ABS or PLA for structural printed parts?

TL;DR Is ABS a better material to use for structural parts of a 3D printer, as opposed to PLA? I have been looking at various suppliers of printed parts for a Wilson II, on eBay. One supplier ...
38
votes
5answers
4k views

How is PLA different from ABS material?

What are the main differences when using ABS over PLA and vice versa?
19
votes
4answers
13k views

What to do with failed/unwanted 3D prints?

I am planning on getting a 3D printer soon and I was just wondering, what do you do with 3D prints that either failed or were prototypes that you no longer want? I tried looking online but the closest ...
5
votes
3answers
2k views

Extruder skipping/clicking (brand new printer)

I just got a GeeeTech Rostock 301 mixer head delta printer and am having trouble honing in on why the extruder is struggling with my first spool of ABS. Being the main parts of the printer came ...
6
votes
2answers
13k views

What are the costs per meter of filament for PLA, ABS and PET?

My Craftbot Plus Craftware slicer estimates cost per job based on filament prices I add as parameters. What costs per meter would you use? I created spreadsheets to calculate this for 1.75mm ...
6
votes
3answers
999 views

Printing Object in multiple parts

Is there any software/methods to automatically splice objects into multiple pieces sort of like a jig saw puzzle so that I can combine them together and bypass the build plate size limit? As an ...
3
votes
1answer
2k views

What's smoother? Acetone treated PLA or ABS

From my understanding, both PLA and ABS can be treated with acetone to make them smoother. So when they are treated with acetone, which is smother PLA or ABS or are they about the same? When I ...
14
votes
6answers
11k views

Safety precautions when using acetone

Acetone can be used to smooth ABS prints. What safety precautions should be taken during its use?
11
votes
3answers
4k views

How can I stop my print bed tape from sticking to the filament?

I made a test print for a small gear (~ 1.5 inches in diameter) a few months ago, with a hole through the center. On the first try, the filament (ABS) fused to the print bed, meaning that I had to ...
3
votes
2answers
242 views

What do you recommend for removing prints from Monoprice Maker Select bed?

I've been making some ABS prints, but it's really hard to remove it afterwards. I've read a lot of different ways of removing it, including using the included chisel/spatula, using air duster, 50/50 ...