Questions tagged [abs]

Use this tag for questions on Acrylonitrile Butadiene Styrene, also known as ABS, a commonly used thermoplastic polymer.

Filter by
Sorted by
Tagged with
3
votes
3answers
162 views

Help printing in ABS

My first attempt to print in ABS has been an unmitigated disaster, and I could do with some advice before I try again. I've been trying to print a Bean Hopper Extension for Melitta Barista TS Smart ...
0
votes
2answers
36 views

Up! mini raft sticking to prints

I have an UP! mini and I am using the UP Studio and ABS 1.75 mm. My prints are always stuck to the rafts and are impossible to remove without destroying the print. I've had a look at the settings on ...
1
vote
0answers
22 views

Printing issues of ABS on a Flashforge Adventure 3 nozzle blocked

I tried to print in ABS for my first time. I have had my printer for almost 2 years but have only just started to use it and have a total of 28 hours of print time. The job I tried to print was meant ...
8
votes
4answers
13k views

ABS or PLA for structural printed parts?

TL;DR Is ABS a better material to use for structural parts of a 3D printer, as opposed to PLA? I have been looking at various suppliers of printed parts for a Wilson II, on eBay. One supplier ...
0
votes
0answers
34 views

Unwanted texture at base of ABS print

I'm getting close with this print, but I'm seeing some rippling at the base that I can't seem to eliminate (see photo at the end of the post). The model is here if it helps. It seems that the texture ...
1
vote
1answer
197 views

How to switch from PETG to either PLA/ABS mid print?

I have an Ender 3 Pro and I'm about to print a relatively large model on it. I've been printing in PETG and I'd like to use up the last of the roll during this print. When the roll runs out however, I ...
2
votes
2answers
832 views

Making Polyurethane molds with PLA (or ABS) 3D printed master

I want to make Polyurethane molds for concrete using 3D printed PLA or ABS master object. like this video: (this video is not about concrete of course!) I'm not sure ...
1
vote
1answer
564 views

Which 3D printer should I use to make custom miniatures for a tabletop game?

I would also be curious on how I could get the best results with these printers. I am in a situation where I have cheap access to a: Fortus 250mc, which prints in ABS and has a minimum resolution of ...
1
vote
1answer
113 views

How to set multiple draft shields in Prusaslicer?

Draft shields helped me a lot to get some usable prints out of ABS on a non-enclosed printer with a small printing bed, but I noticed that the shield cracks (it is affected by the issue that would ...
0
votes
0answers
31 views

Enclosures (w.r.t. emissions) useful for not only printing ABS?

I've been reading and seeing a lot of texts on the internet and videos on YouTube claiming that enclosures are both beneficial and not so beneficial. My main concern though is the possible toxic fumes ...
2
votes
1answer
53 views

Are there differences in filament consumption between ABS and PLA

I have been printing the same model once with Verbatim PLA and once with an ABS material from Switzerland. For both I was using two brand new 1 kg spools of filament. I was printing both at the same ...
3
votes
3answers
164 views

How to solve ABS deformation at the bottom?

I am printing small mechanical pieces in ABS: 100 ºC bed temperature 70 ºC Room temperature 250 ºC nozzle temperature 0.4 mm nozzle, at 0.15 mm per layer. 100.8 % scale to compensate ABS dimensional ...
19
votes
4answers
13k views

What to do with failed/unwanted 3D prints?

I am planning on getting a 3D printer soon and I was just wondering, what do you do with 3D prints that either failed or were prototypes that you no longer want? I tried looking online but the closest ...
1
vote
1answer
50 views

How to prepare bed for printing ABS filament?

I have never used ABS filament before, so my question is, how do I prepare my glass build plate for printing ABS filament? My second question, is, after you have prepared it, and have finished ...
1
vote
1answer
59 views

Is nozzle no longer heating up correctly related to hotend insulation being pulled off?

The insulation of the heater block got pulled off... I was trying to print ABS on my TEVO Tornado, overnight. But I not-so-smartly left the window open overnight, thinking it was alright (as to remove ...
7
votes
4answers
7k views

Raft hard to remove?

I've been having a hard time lately getting the raft off of my ABS prints. Is that a symptom of either a nozzle or bed that are too hot? Or is there some other factor I should be looking in to? I ...
1
vote
0answers
87 views

Consistent blobbing and gaps in print towards right side

Issue: I'm having a problem with some blobbing and gaps consistently in the same areas. The left edge is always good, the right edge is very bad (especially around the corner) and the front and back ...
2
votes
0answers
67 views

Prusa MK3S Nylon&ABS print failures

I'm using Prusa i3 MK3S and every time I want to create a durable, impact resistant part, I use ABS/Nylon. The problem is, however, that when I print something small (of less than 1 cm width for ...
1
vote
1answer
250 views

3D Printer does not print whole object

Just took delivery of a massive Anycubic Chiron to my house and have been trying to get it printing successfully for supplies for fellow clinic staff. For some reason, it is only printing a portion of ...
0
votes
1answer
80 views

Why can't I use PLA with ABS in a dual extruding 3D printer?

I have a XYZ Da Vinci duo and I want to run water soluble PLA with ABS How can I do that?
6
votes
3answers
560 views

Is 3D printing feasible for a coaxial rotational joint?

In a design that I need to prototype, I have a coaxial, rotational joint between 2 cylinders connected to another coaxial rotational joint between 2 cylinders by a hinge. I have attached the ...
3
votes
2answers
871 views

Best way to fix ABS corner curling on enclosed Prusa style printer with PEI heatbed?

I'm trying to set up an enclosed (custom enclosure) Prusa i3 style printer for ABS, but having a fair amount of difficulty preventing the part corners from curling. Detailed specs: Geetech A10 (...
2
votes
3answers
1k views

Printer changing temperature after selecting file

I have just got a Monoprice Maker Select 3d printer (which is really just a Wanhao Duplicator i3). I want to print a model that came on the included SD card (...
3
votes
2answers
248 views

What do you recommend for removing prints from Monoprice Maker Select bed?

I've been making some ABS prints, but it's really hard to remove it afterwards. I've read a lot of different ways of removing it, including using the included chisel/spatula, using air duster, 50/50 ...
2
votes
0answers
178 views

Filament change (M600) causes color mixing despite excessive purge

I have an Anet A6, where I uploaded Marlin 1.1.9, because the manual filament change on the stock firmware was really bad (90 % of the times it clogged the hotend). I've tweaked it a bit, and I'd ...
2
votes
5answers
6k views

Printing temperatures for ABS on a Flashforge Adventurer 3

I've recently acquired a Flashforge Adventurer 3 and am having difficulty printing with ABS. The initial layers seem to lay and stay pretty well, though after a few more moments, one side will peel up ...
5
votes
4answers
2k views

Weird ripping and warping of ABS print

I print my ABS at: 240 °C; with a bedtemp of 80 °C; 5 % rectilinear infill; 0.25 mm layer height; 2 solid layers top and bottom; Fan is completely disabled; 0.25 mm extrusion width; 50 mm/s ...
3
votes
1answer
53 views

Acetone Smoothing an ABS Cone - (New to 3D printing)

Today marked my first time using a 3D printer - have to admit I was originally skeptical but am now incredibly impressed and am having to hold myself back from purchasing one for myself! Was a great ...
1
vote
1answer
1k views

Nail polish remover that won't dissolve ABS?

In Finishing sunken text in 3D prints, I found that nail polish works great for filling sunken lettering in 3D-printed parts, but the procedure for using it requires removing the excess from the non-...
2
votes
2answers
2k views

What causes these blobby corners

Contrary to a lot of other corner related problems (where the corners are bulging), I seem to have a different problem where the corners (ONLY) seem to stick out and appear blobby in the x/y plane. ...
2
votes
1answer
96 views

What kind of paint and varnish can be used with ABS?

I know that acrylic paint, the same kind that is used to paint miniature figurines, works best for PLA. Does it works on ABS pieces as well? Can I also use the same kind of varnish that is used for ...
6
votes
4answers
25k views

How many grams will be used in a print

I have an STL file and I would like to know how many grams would this print consume. Is there a software so I can get it or an online link that can say me that?
4
votes
3answers
551 views

Looking to use 3D printing to make a master plate for rubber stamp vulcanizing

I am an art rubber stamp maker, using a vulcanizer to make art rubber stamps from molds that are usually created with a magnesium plate. The normal process is to send artwork off to an engraving ...
3
votes
5answers
129 views

3D Print Enclosure

Developing an electronic product for which I'll need an enclosure. It's about 50x30x20mm and should survive higher temperatures (50-60 degrees). Because of the low volume (under 500 required per year),...
2
votes
2answers
1k views

ABS de-layering on Ender 3

I feel like I’ve tried everything. I’ve had an Ender 3 for seven months now printing in PLA. I’ve modded it plenty including BLTouch. I’m now doing a project that really requires ABS so I have the ...
4
votes
3answers
841 views

Increasing rigidity of curved, long, thin parts

I'm attempting to model and print a globe. The semi-circular arm that holds the globe has an outer diameter of 98mm and inner diameter of 92mm, so the arm is fairly thin. The arm has a small hole on ...
5
votes
2answers
8k views

Is there a way to print with ABS without enclosure?

ABS is a very strong material, but it also has some downsides. One of them, which is the necessity of having a printer with enclosure, completely discouraged me from using it, as it would be a waste ...
7
votes
3answers
1k views

How to minimize damage when removing an ABS print from a heated glass print bed?

Usually it will either will rip the tape, or break the print somehow. Currently using ABS on a taped glass bed with a layer of hairspray for adhesion.
6
votes
2answers
13k views

What are the costs per meter of filament for PLA, ABS and PET?

My Craftbot Plus Craftware slicer estimates cost per job based on filament prices I add as parameters. What costs per meter would you use? I created spreadsheets to calculate this for 1.75mm ...
4
votes
5answers
4k views

Best method to make dissolvable supports?

Sometimes supports are very difficult to remove (physically) when I print with ABS. The image below, from Thingiverse - MOF-5 unit cell, is after significant effort to remove the yellow ABS supports ...
0
votes
1answer
409 views

Good profile for slicing ABS in Slic3r?

Does anyone know of a good slicer profile (i.e., an .ini file.) for Slic3r for printing ABS for a Prusa i3 MK3S printer?
14
votes
6answers
11k views

Safety precautions when using acetone

Acetone can be used to smooth ABS prints. What safety precautions should be taken during its use?
11
votes
4answers
6k views

Layer delamination

I've printed mostly ABS in the past and encountered delamination between layers many times. I've ensured the following conditions regularly: Build plate is level Base of print isn't warped (using ABS ...
7
votes
5answers
1k views

“Tac Tac” sound when printing with ABS

My 3D printer makes weird sounds. When it's at >75% printing speed the extruder motor makes a "tac tac" sound and it goes backwards, pushing the filament back, for a small interval of time. I have ...
5
votes
4answers
3k views

How thin can I make the wall of a pipe?

For a science project, I'm 3D-printing some custom pipes and tubes to regulate the flow of gas (a combination of ethyl alcohol and water vapor) through an apparatus. They need to be pretty small, as ...
17
votes
7answers
4k views

What can I use to “sand” my ABS prints?

I have a 3d printer that uses ABS filament. The software I use will generate vertical supports for my objects before printing that can be easily broken off after they have been used during print to ...
2
votes
1answer
983 views

How to paint ABS to look like wood [closed]

I have a piece printed in white ABS, which is a half-scale replica of an unvarnished oak sculpture. After sanding off the worst of the layer lines, I'd like to paint it to get a nice wood finish. I ...
1
vote
1answer
241 views

FDM, ABS Post-processing methods

I have built a few parts that have printed 'pins' on them (2mm diameter 1.5 cm length). Due to the orientation that the build requires the pins have to have support material on them. (The part has to ...
6
votes
3answers
1k views

Printing Object in multiple parts

Is there any software/methods to automatically splice objects into multiple pieces sort of like a jig saw puzzle so that I can combine them together and bypass the build plate size limit? As an ...
4
votes
2answers
1k views

3D printer filament will not load after running the printer out of filament

We wanted to test the post process properties of PVA but did not want to print anything. We unloaded the ABS that was in the printer and then started loading some PVA. After the PVA was loaded we ...