Skip to main content

Questions tagged [anycubic-kobra-max]

The tag has no usage guidance.

Filter by
Sorted by
Tagged with
0 votes
1 answer
2k views

Print in the first layers keeps failing on new Anycubic Kobra

I'm not new to 3D printing, but I have always used resin 3D printers. Now I have bought an Anycubic Kobra and I'm trying out ABS. I can't figure out what I'm doing wrong, I have tried many different ...
user3161330's user avatar
2 votes
2 answers
650 views

How do I avoid straight lines for walls in Cura?

I need to print a thin piece. Theoretically, it could work, but Cura prints the walls as single lines. In my case, it is just this line that breaks apart as you can see here. Is there a setting that ...
tmighty's user avatar
  • 541
4 votes
1 answer
169 views

What are these defects caused by?

I am printing PETG with my Kobra Max. Material: ERYONE PETG Filament 1.75 mm The recommended print settings are 220-240 °C. I am using a nozzle temperature of 230 °C and bed temperature of 70 °C. Can ...
tmighty's user avatar
  • 541
0 votes
2 answers
1k views

Some kind of stringing

I experience some lines on my prints. However, I would not really call them "stringing". I have seen some stringing and it was rather like an undefined spider web. But the lines that you see ...
tmighty's user avatar
  • 541
1 vote
0 answers
297 views

How do I choose a nozzle for PA12+CF for Kobra Max?

I am sorry if I sound too newbie, but to me, it seems like an unsolvable riddle: I have not yet used any other nozzle than the one that comes with my printer. I would now like to print Fiberlogy Nylon ...
tmighty's user avatar
  • 541
7 votes
2 answers
2k views

A vertical scar on the print surface, what is the name of this problem?

Printer: Kobra Max Nozzle: 0.4 mm Material: PLA Slicer :Cura I have printed 1 model 3 times with different settings (different temperatures and different bed temperatures). Try 1: 190 °C / 50 °C Try ...
tmighty's user avatar
  • 541
4 votes
4 answers
2k views

What is this called and how do I avoid it? (model frees itself from support structure and warps upwards)

I want to print the following model on my Kobra Max using ABS. I have uploaded it here. I have tried it 3 times now, it always results in this: As you can see, one part managed to break free from ...
tmighty's user avatar
  • 541
2 votes
1 answer
121 views

Are magnetic hotbed plates interchangable?

The Anycubic Kobra Max comes with a glass plate. I need to use a textured PEI plate for my Kobra Max. As I understand it, the PEI plate needs to be used on a magnetic bed plate. Currently, there is no ...
tmighty's user avatar
  • 541
2 votes
1 answer
421 views

Rough surface coated PEI textured build surface to fit Anycubic Kobra Max?

I have an Anycubic Kobra Max. It has a bed size of L430*W410. I would like to print a rough surface as shown here: To do that, I need a coated PEI build plate, and I need to print the surface ...
tmighty's user avatar