311 views

How to remove ABS from PEI Sheet

Recently building a new printer, I went with a Wambam PEX system. When I began printing ABS I found it did not stick very well and eventually purchased a new build plate and a PEI sheet since PEX isn'...
8
votes
3answers
697 views

How can you prevent the build plate from slipping?

I have just set up my new 3D printer. However, the build plate keeps slipping while printing. I tried to use binder clips to keep the plate in place, but this makes the build plate unlevel, messing up ...
1
vote
1answer
84 views

Will glue sticks form a barrier on a build surface to prevent PETG from damaging the surface?

Will glue sticks, such as Elmer's All Purpose, Cra-Z-Art washable or Scotch Permanent, form a barrier on a build surface to prevent PETG from damaging the surface? While forming a barrier that holds ...
1
vote
1answer
835 views

What is the best build surface for PETG?

This question doesn't necessarily have one answer. I'm looking for a build surface that doesn't tear up when removing the PETG print, but still holds the PETG down and keeps it from warping. I am ...
0
votes
0answers
17 views

How well does a polyimide build surface work with PETG?

I've noticed that PETG releases well from polyimide tape and wonder how well it would work for a build surface. My concern is PETG may not stick well enough to polyimide.
1
vote
1answer
2k views

Resin printer build plate scratches/ damage

I have an anycubic photon, and occasionally have trouble removing prints from the build plate. While trying to removing prints I've put some scratches into the surface, as I guess I've come in at the ...
1
vote
1answer
79 views

Paper as build surface - how will that work?

I have a Creality Ender 3 that needs a build surface (both the build-tak sticker and the removable stiff backer). My dad has been pestering me to try using paper as a disposable surface. I am hesitant ...
2
votes
1answer
73 views

Ender 3 build surface is sticking up in the middle

I have had my Ender 3 for a few months now and have loved it! I recently noticed that the build plate, the black removable part of the print bed, is sticking up in the middle. If I poke it, it goes ...