5k views

Bed too close to nozzle?

I've been having some bed adhesion problems that I have been trying to solve by leveling the bed. I think that it's pretty level now but when I start a print the lines seem pretty flat. Is this true? ...
2
votes
1answer
2k views

Stepper motor for CR10-S5 Y-axis

I need to replace this stepper motor with the following product identification: It’s a Y-axis for CR10-S5 and labeled as JD42HS60-1500A-02F. What type of stepper motor is this?
1
vote
2answers
3k views

Proper wire gauges for extending all CR-10S wires

I want to extend all my CR-10S wires. I have two long wire types: 22 and 18 AWG wires. I've done some research and found the following: Extruder heating element: 22 AWG or lower. Extruder thermistor ...
1
vote
1answer
262 views

Free UARTs TX and RX pins on CR-10S motherboard

I have a WiFi module that only needs two wires connection to work. These are RX and TX pins connected to Arduino or the CR-10S printer board but I don't know if there is any physical or software UARTs ...
1
vote
1answer
2k views

Is endstop / z-probe wire required for BLTouch installation on CR-10S

I am confused about installing BLTouch on CR-10S. This is my motherboard: Below is a screenshot for the wiring of the BLTouch sensor: See the circled sections in yellow. Notice that the Z- socket ...
4
votes
3answers
479 views

Which capacitor to change on CR-10S S500 motherboard?

I have a CR-10S 500 and want to change a capacitor on it to improve and solve temperature issues. This capacitor that needs to be changed should be labeled as "C4" as mentioned on this post but it's ...
1
vote
1answer
610 views

Creality CR-10 slightly jerks when moves from right to left

So when CR-10 prints square (like on the video starting from 6 second) while being in the top right corner extruder jerks i.e. slightly moves to the right and then continues movement to the left. So ...
9
votes
3answers
3k views

Filament isn't going into the Bowden tube, instead it goes “into the room”

The pictures explain my problem. I have already tried to reduce the retraction but that showed no effect. Thank you for your help. The effect is a total stop of the print (no material is extruded). ...
5
votes
2answers
2k views

Creality CR-10 Clogs and Underextrusion - Filament at fault?

I've been printing successfully on my CR-10 for the past year now. I've had issues now and then but have been able to look around the internet and solve them. I've been using some Flashforge white PLA ...
3
votes
2answers
3k views

What are the specifications of the dual voltage controller of the Ender 3/CR-10?

Following on from What level of voltage does the Creality Ender-3 run at? Dave's answer states that both 12 V and 24 V can be used on the controller board. It also goes on to say that the ...
7
votes
2answers
2k views

Nozzle heats up past the setpoint and increases

I made a few successful prints since I got my CR-10 two weeks ago and I didn't run into any major trouble. The printer is new. Today I set it to "preheat" mode while I was preparing the SD card with ...
0
votes
3answers
150 views

Finding a reputable seller for CR-10S

After doing a lot of research, I've decided I want to purchase a Creality CR-10S as my first 3D printer. I'm trying to locate a reputable, local seller. Other than Amazon, which seems to have a bit of ...
11
votes
7answers
1k views

Noise Reduction

I am looking for methods to reduce the amount of noise produced by my CR-10. I have the printer in my downstairs study and if I'm doing a long print job, you can hear it upstairs in my son's bedroom ...
4
votes
1answer
3k views

Low Filament Sensor for Creality CR-10? [closed]

I have been playing with my CR-10 for about a month now and I was wondering if there is a low filament sensor available for the CR10. I found this listing on Amazon, Creality 3D Printer CR-10 S4 ...
5
votes
2answers
19k views

Setup Creality CR-10 in Cura

Can anyone help me find/confirm the information needed to setup the CR-10 in the Cura Software I have following settings from research: Printer Settings x = 300 mm y = 300 mm z = 400&...

1
2