Questions tagged [delamination]
Questions relating to the type of print failure that causes the layers to separate from one another.
10
questions
2
votes
0
answers
68
views
Walls separating only on one side of print bed
Whenever I print, the walls separate when genial pressure is applied, this only happens to one side of the print, the side that faces the rear of the printer. I'm using 5 walls, so it’s only truly ...
4
votes
0
answers
203
views
Perimeters/shells not properly fusing - delamination
I come to you all in my time of need, as I have nowhere else to turn. I’ve been a 3D printer for about two years now. I have an Ender 5 Plus.
Up to this point, all of my prints were fine straight out ...
5
votes
3
answers
419
views
Help printing in ABS
My first attempt to print in ABS has been an unmitigated disaster, and I could do with some advice before I try again.
I've been trying to print a Bean Hopper Extension for Melitta Barista TS Smart ...
2
votes
1
answer
291
views
Delaminating in the middle area of photon printer
I've been getting delaminating and other issues in the middle area of my Anycubic photon printer.
Sometimes the print won't stick to the print bed and sometimes it delaminates like in the images below,...
1
vote
1
answer
273
views
How to set multiple draft shields in Prusaslicer?
Draft shields helped me a lot to get some usable prints out of ABS on a non-enclosed printer with a small printing bed, but I noticed that the shield cracks (it is affected by the issue that would ...
1
vote
2
answers
2k
views
Delamination in resin prints
I have observed some occasional delamination in horizontal layers of my resin prints — see two examples:
What is the cause, and how can this be minimized?
2
votes
2
answers
1k
views
Delamination issue Ender 3 Pro PLA
I recently bought some SUNLU PLA black filament and was attempting a small print with it and it started to come out in strings and lumps and was incredibly inconsistent. Before this I'd been using ...
3
votes
3
answers
2k
views
Print is not properly laminated at certain height
I have a Wanhao Duplicator i3.
I have done many excellent prints with this printer, and have first hand experience that it can do a pretty much flawless print.
But... Recently, I am experiencing ...
5
votes
4
answers
4k
views
Hatchbox Silver PLA settings?
I have a RepRap Prusa i2. I have done the majority of my printing with clear PLA that I got on the cheap from eBay. It works just fine.
I bought a roll of Hatchbox Silver PLA (1.75 mm) from ...
11
votes
4
answers
6k
views
Layer delamination
I've printed mostly ABS in the past and encountered delamination between layers many times. I've ensured the following conditions regularly:
Build plate is level
Base of print isn't warped (using ABS ...