0answers
53 views

3D print Ember Autodesk issues affect print quality

does anyone know something about Autodesk Ember print issues? Currently I am working on my master thesis and I would like to print with the Ember 3D printer a holder (see attachment) using the ...
1
vote
1answer
138 views

Top-Down SLA Printer Bulging Issue

I have designed and built a top-down SLA 3D printer that uses a 405 nm 500 mW laser along with some galvanometers. I filled the vat with glycerin and then topped it off with about 2.5 cm of resin. I ...
1
vote
0answers
31 views

Large SLA Build Plate