Prusa i3MK3S+ layer skip with polycarbonate (overheating?)
On the last couple of polycarbonate prints with my Prusa, one or more layers have been completely skipped (i.e. no material extruded). The rest of the print is fine save some minor warping. I'm ...
0
votes
0
answers
164
views
Anycubic Vyper filament loading problems
I recently acquired the Anycubic Vyper, and it's been working fine, until a few days ago. The filament extruder stopped working properly, as in it would extrude an amount of filament, before making a ...
1
vote
1
answer
56
views
Filament Spool Stalls Extruder Motor Destroying Print
I am having the frustrating problem where my extruder motor starts skipping steps and stops extruding simply because my filament is wound too tightly. There are some parts of my filament that are so ...
3
votes
2
answers
159
views
Filament Jamming in Hotend. Why?
This has me stumped. I had been printing normally until this happened. Below is an expurgated version of my headache over two days. Some help would be appreciated.
Printer is Hypercube Evolution (...
0
votes
0
answers
79
views
E3D V6 hotend gets jammed very frequently
In the past couple of weeks, my V6 hotend gets jammed very frequently. The nozzle is 0.4 mm and the printer is a D-Bot.
Here are some of the things I have tried so far,
Switched between the original ...
2
votes
2
answers
369
views
PLA Jamming- is the heat break too hot or too cold?
I’m getting nothing but jams with a new BCN3D Sigma R19 printer, printing PLA at 195 °C, two brands (BCN’s own brand and Monoprice orange). 6.5 mm retraction, as used in BCN’s PLA profile. Using their ...
2
votes
1
answer
264
views
Filament getting stuck/nozzle is clogged
For some reason on my Raise 3D N2 plus with a Bondtech-Extruder I am sometimes seeing filament jams and sometimes it prints without any issues. I am using PLA at 215 °C.
When the filament is jammed I ...
1
vote
3
answers
337
views
Filament jam on the tube entrance
I have a problem in regards to filament jam, however I don't think that my case is any related to the extruder nozzle.
After 30 to 40 minutes printing my filament bends and get stuck on the tube ...