Questions tagged [glue]

Bonding two or more items together, where at least one is 3D Printed.

Filter by
Sorted by
Tagged with
23 votes
4 answers
59k views

What glues for bonding printed PLA to injection-molded plastic?

I will be creating a small tube styled piece to use as a junction between two pieces of plastic. The idea is to reattach the two pieces and provide strength so they don't break apart again. I plan on ...
5 votes
3 answers
3k views

What glues to use for PETG?

In analogy to: What glues for bonding printed PLA to injection-molded plastic?, what are the best glues to use for PETG? I mostly print in PETG and have occasional failed prints which I usually ...
  • 31.4k
2 votes
2 answers
261 views

How can cyanoacrylate haze be removed from PLA?

Using cyanoacrylate to glue PLA parts sometimes leaves a white residue or haze near the glue locations. Is there an easy way to remove it? I've tried water and alcohol swabs but after drying the haze ...
  • 300
0 votes
1 answer
76 views

What is the best glue for the task of assembling a 3D printed part with other materials?

I have printed some connectors from PLA, in order to make a frame for a "tent" cover for my Ender3 printer Since printing rods would be a long process with likely poor results, I'm using ...
  • 855