2
votes
0answers
64 views

Weird solid infill for chamfer

I am very frustrated with some weird solid infill issue, mostly due to sloped wall such as chamfer for fillet. Here is an example. I have a 20x20x20 mm cube with 2 mm rounded chamfer at the ...
2
votes
0answers
325 views

Best infill for inter-layer adhesion

I'm fairly convinced that gyroid is the best infill for a lot of purposes, and use it regularly now, but both conceptually and anecdotally, it doesn't seem very good for reinforcing inter-layer ...
1
vote
1answer
87 views

Why does infill percentage stop the print from sticking to the bed?

I've recently purchased an Ender 3 and have had great success with some Cura settings found on a YouTube Tutorial at 0.2 mm resolution. So then I noticed that there were default settings in Cura for ...
0
votes
1answer
63 views

Problem with grid infill (line positioning)

I have a problem with the grid infill on my BCN3D+ Dual Paste extruder: when I print a structure the lines of the infill are not evenly printed, every two lines the gap between the lines is higher (...
0
votes
1answer
156 views

Infill not printing well. What I am doing wrong?