G-code to get the 3D printer to shake resin bubbles off from a casting
While this is not directly 3D printing related, I intend to use my 3D printer (Labist's ET40) to shake air bubbles off of a resin casting.
I printed parts, made a mould of them in silicon, then cast a ...
2
votes
1
answer
733
views
Labists ET4 printer nozzle hits bed after automatic levelling
I use Slic3r to create G-codes for my Labists ET4 printer. Usually, no problem.
Now, as soon as I tried to start a print, the nozzle head went down as usual, but this time it went a bit lower than 0 ...