Questions tagged [nylon]

For questions regarding Nylon filament

Filter by
Sorted by
Tagged with
1
vote
2answers
81 views

How does direct drive conversion allow higher print temperatures?

I have an Ender 3, currently in stock Bowden extruder configuration. I want to be able to print nylon and TPU, both of which require temperature too high for the tolerance of the PTFE Bowden tube (as ...
3
votes
1answer
78 views

Do hygroscopic filaments (PVA, Nylon) absorb moisture while in a heated enclosure

I’m new to using PVA support filament, and have read it is especially prone to absorbing moisture out of the atmosphere. People made it sound like it starts to happen quickly, and if you aren’t ...
3
votes
1answer
71 views

Is it better use Nylon fillement for cold pull even if I have been using PLA?

Using Prusa I3 MK3S I am using PLA fillement and I need to do cold pull from time to time. I noticed many people on Internet suggestusing Nylon fillement for clod pull. I wanted to reach out to this ...
1
vote
1answer
146 views

How to set multiple draft shields in Prusaslicer?

Draft shields helped me a lot to get some usable prints out of ABS on a non-enclosed printer with a small printing bed, but I noticed that the shield cracks (it is affected by the issue that would ...
1
vote
1answer
170 views

Increase hotend temperature on Monoprice Ultimate 2

I'm fairly new to 3D printing and I have a Monoprice Ultimate 2. The Monoprice website says it can reach 250 °C with a 100 °C bed temperature. I want to print some projects using Matterhacks Nylonx, ...
2
votes
3answers
346 views

Does a teflon insert in an E3D V6 clone limit it's useable temperature so it can't print nylon?

I'm new to this game, and recently upgraded the hotend on my Ender 3 Pro to a clone of an E3D V6, as I'm keen to do nylon prints at some point. I noticed however that this one I got has a teflon liner ...
1
vote
1answer
695 views

Any experience with nylon drying on heated build platform and printing on paper?

A while a go I thought that I could try printing in Nylon on my Wanhao Duplicator i3 with full metal hotend. Boy, was I wrong: The filament was not dry and popped like foam. The platform (Buildtak) ...
2
votes
0answers
75 views

Prusa MK3S Nylon&ABS print failures

I'm using Prusa i3 MK3S and every time I want to create a durable, impact resistant part, I use ABS/Nylon. The problem is, however, that when I print something small (of less than 1 cm width for ...
1
vote
1answer
185 views

Printing with Nylon 6,10

Can Nylon 6,10 be used for 3D FDM printing? What range of temperatures be used to print with it? How does it compare to the standard 3D printing Nylon material (I think it is 6,6).
5
votes
2answers
131 views

What are the limiting factors when trying to print flexible filaments with a Bowden extruder setup?

Other than the most obvious issue with the filament kinking in the tube, what other issues could arise when trying to print flexibles (i.e. TPU/TPE, Nylon, etc.) with a Bowden style extruder setup? ...
0
votes
1answer
113 views

Settings for Taulman 618 Nylon

I would like to know what are the best settings for Taulman 618 Nylon filament? In particular, the print head and print bed temperatures.