2
votes
1answer
253 views

Will there be any negative effects on the print process if the printer is outside?

If I buy a printer, it will be going on a small table on a front porch so as to keep the smell from the house. The porch has a roof, so precipitation is not a concern. I will find a way to keep the ...
21
votes
5answers
57k views

Which is more durable to sunlight/weather - PLA, ABS or PETG

The backstory: I'm installing a pigeon net in my home. Because of the shape of the opening I'm installing the net in and the material on the sides it's difficult to anchor the net using the normal ...
11
votes
2answers
16k views

PLA use outdoors?

I have been using PLA filament for two years now and have had good prints. ABS on the other hand has not been so good, so my choice of filament is PLA. I am getting ready to do a sign for the ...
16
votes
6answers
13k views

3D printing for outdoor use: "What types of filament are most weather resistant?"

I'd like to print modifications for my bird feeder, both to patch over the hail damage from last summer and to try to deter the neighborhood squirrels. I have an FDM printer (and experience with ...