0answers
1k views

Horizontal defects when linear_advance enabled?

What could cause that? When linear_advance (v1.5) is "off" (M900 K0) - everything is uniform and smooth, only corners are protruding as expected. When it is "on"...
1
vote
1answer
178 views

Problem printing bigger models in the Ender 5

In all the bigger prints I print on my Ender 5 with PETG I have problems with warping and raft detachment during printing. I have a glass bed and I'm using Ultimaker Cura 4.6.1 standard printing ...
0
votes
0answers
15 views

How to stop stalagmite formation with translucent PETGs

I have had this issue with both Sunlu PETG (red) and TechnologyOutlet PETG (blue), both are translucent PETG filaments. This is printed with a bowden setup, 5 mm retraction, 85 °C bed and 245 °C ...
0
votes
0answers
9 views

How well does a polyimide build surface work with PETG?