14k views

Why keep the bed heated after initial layer(s) with PLA (or PETG)?

I'm printing on an Ender 5 with the default flex/magnetic build surface. I read that PLA and PETG may sometimes be printed without any bed heating at all and also that bed heating is the main ...
9
votes
3answers
8k views

PETG Collecting on the Extruder

I have recently bought a spool of eSun PETG. So far I really like the filament. My only complaint is, I get lumps of charred filament deposited on my object. The slicer I used is Craft Ware and I have ...
8
votes
3answers
14k views

PETG layer adhesion

I've been playing around with PETG for the first time, and everything seemingly worked right just from the start - clean prints, no stringing, no bed adhesion problems, no warping or dimensional ...
6
votes
2answers
299 views

Thermal Runaway E1 at Layer 2

Before I start, I'll give you my setup: Ender 3 Pro Marlin 2.0.7.2 Material/Nozzle: PETG 0.4 mm @ 215 °C Bed: Glass @ 80 °C Default printing speed: 70 mm/s Standard part cooling fan Since I've ...
6
votes
1answer
5k views

Question about retraction distance and stringing/print quality with PETG

I've tried printing the Basic Stringing Test on my CR-10S using PETG (250 °C nozzle, 80 °C bed) with different retraction distances leaving all the rest unchanged. In the image below you ...
6
votes
3answers
3k views

Messy top layer with PETG filament?

I'm having issues getting PETG to print nicely. I have encountered pretty much every issue because when I fix one thing another issue pops up. I see people saying that you should "just copy your ...
5
votes
6answers
12k views

How to work with PETG? Settings, caveats, etc

We've been doing some printing with PETG filament on Ender 3 Pro printer and the result were awful: Here are settings we used: Extruder: 240 °C Bed: ~70 °C (± 10 °C)...
5
votes
2answers
4k views

PETG filament doesn't stick reliably to fake Buildtak surface

I just got my first spool of PETG and tried to calibrate an Ultimaker Cura profile for it on my Ender 3 today with limited success. I've had severe issues with the filament not sticking to the build ...
5
votes
1answer
1k views

Does PETG fade in the sun?

I'm looking at scanning in a statue on my pond and making a print of it. I'm wondering if PETG will fade and how fast. I'm thinking of using white or maybe a bone color if possible. If PETG fades ...
4
votes
2answers
7k views

Can I dry PETG filament under sun?

At the moment the outside surface temperature is around 30 °C. Can I put my PETG spools outside with a fan in order to dry them cheaply?
4
votes
2answers
620 views

PETG grinding with direct drive extruder

I've been wrestling with a filament grinding problem for a few weeks now and I'm stuck. The problem manifests itself as starting a print alright then extrusion stops while the printer keeps moving. ...
4
votes
2answers
1k views

Prusa i3 MK3S 3D printer PETG printing problems

I am using a new Prusa i3 MK3S 3D printer kit. I print lots of things using PLA and PETG. After a week of great performance I noticed that when printing some objects with PETG filament I often ...
4
votes
1answer
1k views

Thermal runaway with specific prints

I have been experimenting with PETG on my CR-10 upgraded with an E3D all-metal hot end and Marlin firmware on the controller. I am printing with 0.8 mm nozzle at 250 °C and an 85 &...
4
votes
1answer
3k views

Bumpy first layer with PETG

When I print with PLA, I get a perfect first layer. However, when I print with PETG, the first layer looks like this: I've read all the info that suggests reducing the temp, speed, and increasing ...
4
votes
1answer
1k views

PETG on Ender 3

I've been trying to print some eSun PETG on my Ender 3 with some questionable results. I am experiencing severe stringing. Attached is a photo of my first layer. My settings are: 250 °C ...
4
votes
2answers
1k views

Under extrusion… sometimes

You can see small gaps in the print which looks like under extrusion (see image below). What is the reason for that? I've tried smaller retracting distances. Temperature looks stable. Print settings:...
4
votes
1answer
131 views

QIDITECH Dual Extruder and PETG

I have just received my QIDITECH printer, I've have ABS, PLA and two reals of PETG. I printed a sample using the clear PETG and this worked find, I didn't have to change any of the default settings. ...
3
votes
2answers
701 views

Can PETG be used as support material for PLA?

Printing supports, either complete, or partially from PVA have not always resulted in successful prints according to my experience with the filament (used in a dual extruder Ultimaker 3 extended). But,...
3
votes
2answers
15k views

Is PETG filament food safe?

I've been trying to find a 3D printer filament which would not release any chemicals if in contact with heated water for a substantial amount of time. So far, I've easily ruled out both PLA and ABS, ...
3
votes
3answers
378 views

Why could my opaque PETG be printing “transparent” in certain places?

I'm printing with opaque grey PETG on glass. The intention is to produce a house number plate, so a shiny, production quality finish on the bottom. For this reason, extruding at 245 °C with a bed ...
3
votes
2answers
324 views

Does acid dissolve PETG 3D prints?

I want to print a lemon squeezer and I would prefer to use PET-G. I don't know if it is safe to use, because lemons contain lots of citric acid. Does it dissolve PETG? I haven't found an answer ...
3
votes
2answers
2k views

Visible lines along Y-axis on Ender 3 Pro

I have a model that's placed on the bed exactly like on this picture: I have constant quality degradation as the bed moves down to print in the upper left corner (1). Everything is fine on the X (2)-(...
3
votes
1answer
353 views

PET-G under-extrusion after changing the nozzle to a 1.2 mm d. one (Prusa i3 mk3s and PrusaSlicer v2.0)

PET-G is the main filament I use. I can achieve high quality of my prints with my Prusa i3 mk3s printer. Recently however, I've recently changed my nozzle from the default 0.4mm to the 1.2mm. I ...
3
votes
3answers
2k views

What glues to use for PETG?

In analogy to: "What glues for PLA?", what are the best glues to use for PETG? I mostly print in PETG and have occasional failed prints which I usually reprint. But what if I'd like to repair a print ...
3
votes
1answer
1k views

Retraction Jamming Problem!

Recently I had this problem where I needed to change filament from PLA to PET-G or similar. And... filament jam. After playing around with different settings and speeds and still getting the same ...
3
votes
2answers
598 views

Why does PETG require slower speed?

PLA has a heat capacity of 1.8-2.1 J/g-K, while PETG 1.1-1.3 J/g-K. This means that each gram of PLA needs more energy to heat up. I assume no "melting latent energy", since we talk about ...
3
votes
0answers
1k views

Horizontal defects when linear_advance enabled?

What could cause that? When linear_advance (v1.5) is "off" (M900 K0) - everything is uniform and smooth, only corners are protruding as expected. When it is "on"...
2
votes
2answers
10k views

PETG Sticking to Nozzle

For a while now, my AmazonBasics PETG filament has been working like a charm. Now, it is balling up on my nozzle. I've tried slowing it down, re-leveling the bed, etc. I don't want to go through the ...
2
votes
1answer
358 views

How to level bed after applying glue stick for bed adhesion

I'm pretty new to printing PETG, and my Creality Ender 3 now has a glass print bed. I've done some research, and it looks like a pretty bad idea to try and print PETG on a pure glass surface for fear ...
2
votes
2answers
1k views

How to solve burnt blobs on Prusa MK3S (PETG)?

As stated above, I am trying to solve a problem I've had for a long time. Unfortunately, this has recently intensified to the point where it causes layer splitting/detaching from each other. I have ...
2
votes
1answer
381 views

Printing with PETG, printer says it's out of filament when it clearly is not

Background: I have an Alfawise U20 (CR10 clone) and am still somewhat of a noob, though I've been learning as much as quickly as time will allow. The Alfawise U20 has "out-of-filament" detection, ...
2
votes
1answer
82 views

Z banding issue

I'm currently facing a Z banding issue that frustrates me more and more. My printer is a modified Anycubic I3 Mega. Customizations: Mainboard: Bigtreetech SKR 1.4 Turbo Stepper Drivers: TMC 2208 v3 ...
2
votes
1answer
3k views

PETG warping - adhesion or temperature too high?

Ender3 v2, SIENOC PETG which advises temperature of 230-250 °C on the box. I'm printing on top of cleaned blue tape, using a temperature of 230 °C for the nozzle and 80 °C for the bed. I've had all ...
1
vote
3answers
11k views

PETG nozzle clearance and extrusion multiplier

I've started printing PETG recently and I'm happy with results so far, awesome strength and good looking (except for stringing). But I've noticed that PETG prints better with more distance nozzle-...
1
vote
1answer
43 views

PETG and Clear Aligner?

There is a material called PETG. In addition, there is a medical solution called Clear Aligner to fix perplexed teeth. Can I use a 3D printer using PETG and make transparent apparatus? The program I ...
1
vote
1answer
156 views

How to switch from PETG to either PLA/ABS mid print?

I have an Ender 3 Pro and I'm about to print a relatively large model on it. I've been printing in PETG and I'd like to use up the last of the roll during this print. When the roll runs out however, I ...
1
vote
1answer
279 views

What is the best build surface for PETG?

This question doesn't necessarily have one answer. I'm looking for a build surface that doesn't tear up when removing the PETG print, but still holds the PETG down and keeps it from warping. I am ...
1
vote
2answers
271 views

MINTEMP BED Fixed error when running consecutive print

I am using "Pretty PETG" along with PrusaSlicer's consecutive print mode. What I am noticing is that upon finishing the first print, the printer hits ...
1
vote
2answers
457 views

How can I add an offset to the first layer to increase clearance?

My printer is calibrated for a certain clearance from the heated bed, which is chosen based on PLA. I would like to try to increase it for the first layer for PETG, so that adhesion is reduced. The ...
1
vote
1answer
62 views

Will glue sticks form a barrier on a build surface to prevent PETG from damaging the surface?

Will glue sticks, such as Elmer's All Purpose, Cra-Z-Art washable or Scotch Permanent, form a barrier on a build surface to prevent PETG from damaging the surface? While forming a barrier that holds ...
1
vote
1answer
214 views

Upgrade hot-end to achieve higher temps (e.g. for PETG)

I'm struggling to get my printer to the temps required for modified PETG (the filament I have is Fillamentum CPE and recommends 255-275 °C), I currently can only reach 245/250 °C even if my target ...
1
vote
1answer
60 views

PET-G grid print problem

My supports 'grid' prints with empty spaces (after stoping extraction over perpendicular lines) (BTW. I have checked the direction when it appears and it has nothing to do with coastig) (the end ...
1
vote
1answer
134 views

Printing Filatech PETG with HyperCube E3Dv6 Clone fails after 3 smooth layers

Recently I got a PETG filament from Filatech to print with my HyperCube printer with E3Dv6 clone Hotend. First 3 layers for every print are pretty fine but 4th layer doesn't stick and my prints fail ...
1
vote
1answer
178 views

Problem printing bigger models in the Ender 5

In all the bigger prints I print on my Ender 5 with PETG I have problems with warping and raft detachment during printing. I have a glass bed and I'm using Ultimaker Cura 4.6.1 standard printing ...
0
votes
2answers
191 views

Difference in weight from Cura to printed model

I've recently switched to PETG , and I'm using Cura as slicer and Ender 3 as printer. I'm printing a model which Cura declares to be 35 g, but if I weigh the printed model it weighs 23 g. I'm printing ...
0
votes
3answers
1k views

What is the best technique to improve removing PETG from the print bed?

What is the best technique to improve removing PETG from the print bed? PETG is known for sticking well to the bed; so well that it does not need a heated bed. If it weren’t for printing other ...
0
votes
3answers
2k views

New PETG spool from eSUN is making popping sound while extruding

I just bought new eSUN PETg filament. When I started to extrude it, I heard popping sound same as moisture boiling out of it. I don't expect new eSUN vaccum sealed filament having moisture content. Is ...
0
votes
1answer
443 views

What material should I upgrade the teflon tube to?

I'd like to print PET on an Ender 3 v2, but I see that some people recommend upgrading the hotend because it will melt the teflon filament feeder tube. I'm not sure if the hotend will even get hot ...
0
votes
2answers
55 views

Apply / find / create a stainless steel coating to apply to a PETG or PLA part to make it react to a magnet

Apply / find / create a stainless steel coating to apply to a PETG or PLA part to make it react to a magnet. My goal is to make a small tubular and conical shapes that can be painted with a stainless ...
0
votes
0answers
15 views

How to stop stalagmite formation with translucent PETGs

I have had this issue with both Sunlu PETG (red) and TechnologyOutlet PETG (blue), both are translucent PETG filaments. This is printed with a bowden setup, 5 mm retraction, 85 °C bed and 245 °C ...