Fixing Z-Hop Stringing

I'm printing a model on my Ender 3 in Mika3D Silk PLA, which (just for reference, this is not atypical) has a stated temperature of 200 °C to 235 °C. I have used this filament before ...
2
votes
1answer
33 views

Print gets worse with every layer - Ender 3

First of all, I'm still new to this 3D printing and I've bought myself a second hand Ender 3 with some mods done to it. I've successfully printed with PLA in different colors. But now the succeeds ...
2
votes
0answers
52 views

Shell detaches from the rest of the part

I'm printing with a Prusa MK3, with the following settings: 3 perimeters 50 % infill infill overlap: 50 % The filament is Polyalchemy emerald green (PLA). Nozzle temperature: 210 °C. ...
2
votes
0answers
78 views

E3D V6 PLA prints leaning / not square

When printing a 1 cm test cube after upgrading to the V6 the cubes are tilted ever so slightly. This does not happen with the stock MK8 hotend, or when printing with the V6 with Polycarbonate+...
0
votes
1answer
14 views

CTC i3 Y-axis thin / no filament deposition

I have this CTC i3 printer; when I print square test prints, as it moves along the Y-axis back to zero (front). It extrudes lines but very thin or none at all. But opposite direction along the Y axis ...
0
votes
2answers
73 views

3D Print something as flexible as a cloth with PLA?