How to recycle filament material from printed parts?

Is it possible to re-use ABS or PLA filament material from printed parts? If so, what is the techniques to reform it?
19
votes
4answers
13k views

What to do with failed/unwanted 3D prints?

I am planning on getting a 3D printer soon and I was just wondering, what do you do with 3D prints that either failed or were prototypes that you no longer want? I tried looking online but the closest ...
18
votes
4answers
3k views

Can I mix ABS and PLA when recycling filament?

I'm thinking of recycling some filament from a couple of recently failed prints. I can reuse them in the future for basic prototypes, so I'm not concerned with whatever weird mixture of colors come ...
13
votes
3answers
1k views

Making your own filament

I"m considering making my own filament, with a device like the one at http://www.thingiverse.com/thing:380987. Partly because it's another machine to build, which is cool, but also to save money on ...
13
votes
3answers
19k views

Uses for PLA scraps

I recently got a 3D printer and have been experimenting with it a lot, resulting in a lot of failed prints (as well as successes, fortunately). I'd like to, if possible, find a way to reuse the ...
8
votes
2answers
4k views

Using the end of a spool

I've seen several Q&As on recycling and reusing plastic from failed prints, but what have you done with the last few meters of filament? I've been keeping the ends of PLA (or sections I needed to ...
7
votes
2answers
1k views

Can I really throw failed PLA prints on compost?

So they say PLA is biodegradable. But I still don't know how much biodegradable. I live in a flat and we have composting trash can in the courtyard. However if I throw PLA in there and it does not ...
6
votes
2answers
350 views

Optimal ratio of fresh to used nylon powder

I am operating a laser sintering machine, using polyamide 2200 powder (with a grain size of approximately 50 micrometers). During a print, a lot of powder goes unsintered and can theoretically be ...
6
votes
1answer
1k views

Finding a shredder for my failed prints

I would love to re-use my failed prints by re-extruding the plastic to be used int he 3d printer once again. One thing that stand in my way is finding a effective way to shred the plastic into smaller ...
3
votes
2answers
309 views

Print paper or cellulose - any recyclable filament?

I know there is a 3d printing technique, where sheet of papers are cut and glued. Like the ones Staples has in their stores. But this sort of paper isnt recyclable, because of the heavy use of glue. ...
2
votes
0answers
30 views

Treating PLA (Polylactic acid) plastic to make it biodegradable

I am using PLA for 3D printing, and I know it does not degrade well in the wild. I would like to know if there is a chemical process I could use to treat it at home. Specifically, I am looking for a ...
1
vote
1answer
282 views

Cleaning IPA with the help of Mercury wash-and-cure?