Questions tagged [robo-r1+]

The tag has no usage guidance.

Filter by
Sorted by
Tagged with
4
votes
1answer
2k views

What makes Pronterface wait for user?

I'm using Cura with the Pronterface UI to slice/print and sometimes printing just stops - always in the first layer - when it happens the printing screen shows "Waiting for user", when I press the ...
1
vote
1answer
1k views

Switch nozzle contact probe auto leveling with Marlin 2.0

I have a Robo R1+ which uses the nozzle contacting the glass print bed to level the printer. When the print head strikes the bed the Z-min endstops open signaling that the bed is touched. I recently ...
0
votes
3answers
345 views

Inconsistent vertical walls on a Robo 3D R1+