Questions tagged [sla]
Questions about the Stereolithography (SLA) method of 3D printing.
8
questions
8
votes
2answers
7k views
Best way to deal with Resin Printers in your living space
I know I did something stupid. I just had to have a SLA 3d printer. The issue being I live in a one bedroom apartment. In the months of owning it I have made lots of amazing pieces, I also for the ...
3
votes
1answer
2k views
Safe way of disposing resin
I have some leftover resin (100 ml) that I`m not planing to use anymore. What is a safe way of disposing it that doesn't involve curing?
1
vote
1answer
283 views
Why is cupping bad in SLA prints?
Why is cupping bad? (I don't mean hollow parts)
Example:
Lets say that I want to print a simple cup without a handle.
There are two obvious orientations:
In one orientation it won't require any ...
1
vote
2answers
635 views
What do I need to go along with my new SLA 3D printer?
I just purchased an Anycubic Photon 3S LCD-based SLA 3D printer. I understand the need for cleaning and curing parts after printing. While the device is in transit, I'm looking to set up a workstation ...
9
votes
4answers
27k views
SLA prints not sticking to build plate
I have been working with our SLA printer (Facture Draken) for a couple weeks now printing in makerjuice waxcast. . I have had some successful prints, but the majority (80%) end up as pancakes stuck ...
2
votes
1answer
343 views
Curated resin size shrink (and methods to reduce it)
I've recently purchased an Elegoo Mars Pro 3D printer.
I've read about that percentage of resin shapes going smaller and I understand that. But are slicers (or software which help with the joints) ...
1
vote
2answers
2k views
SLA resin post-processing: gluing parts together
I've recently purchased an Elegoo Mars Pro 3d printer, and I was wondering when printing large pieces that need to be printed in different steps: is there some kind of post-processing to make it more ...
1
vote
0answers
80 views
Empty patches with a very viscous resin
I have a Mars-like 3D printer, which so far worked very well with typical resins. Then I decided to print a mechanical part with Siraya Blu. I followed their recomendations of a "heavy" support, which ...