Questions tagged [surface]

Questions about the surface of a 3D printed object

Filter by
Sorted by
Tagged with
55
votes
9answers
90k views

How do I give 3D-printed parts in PLA a shiny smooth finish?

The surfaces of my printed parts using PLA plastic look rough and uneven. Would changing filament to a better one make any difference? If not, what kind of methods can I use to achieve a smoother ...
17
votes
7answers
4k views

What can I use to "sand" my ABS prints?

I have a 3d printer that uses ABS filament. The software I use will generate vertical supports for my objects before printing that can be easily broken off after they have been used during print to ...
9
votes
3answers
5k views

Methods for applying full color graphic decals to the surface of a 3d printed part?

I'm trying to find a way of applying graphics to my ABS printed parts. I need a robust method which can produce a decent amount of detail with true color and legible fine text . I also was hoping to ...
9
votes
2answers
4k views

Practical concerns smoothing PLA print with chloroform vapours

One way to give PLA prints a smooth finish is treatment with chloroform vapours (or other solvents, as mentioned in this answer). This method is even featured on Ultimaker website. I would like to try ...
6
votes
1answer
191 views

Triangulation adapted to curvature

I don't know whether this belongs here (where most of the questions appear to be about hardware) or on Math or on Blender (though I've never used Blender). All of the designs that I've published so ...
5
votes
1answer
2k views

How do I give 3D-printed parts in ABS a shiny smooth finish?

The surfaces of my printed parts using ABS plastic look rough and uneven. What methods can I use to achieve a smoother finish for my for 3D-printed objects?
5
votes
4answers
1k views

Is there a way to print on a 3D printed surface?

I have a 3D printed object that I'd like to print on. Adhesive stickers are an option, but as the surface is rounded it's difficult to get a good film to stick well. Is there any system to print on ...
5
votes
2answers
1k views

Bed design for magnetic easy release when printing PLA

I print on a glass bed covered with BuildTak. Prints stick well, release is difficult. They sell a mod, self adhesive magnetic sheet that holds a steel plate which in turn you put the BuildTak on ...
3
votes
2answers
15k views

Rough surface when printing

Is there a specific name for that problem? What causes this, and is there a way how to solve it? Printed with PLA, 2 mm nozzle diameter, 0.2 mm layer height, 20-60 mm/s, 200 °C ...
3
votes
1answer
320 views

Subdivision surface for STL files

How much should I subdivide a surface in preparation for 3D printing? For computer graphics, I know that I need to balance the smoothness and the rendering time, but for printing, I'd like it to be ...
3
votes
3answers
856 views

How to concave a cylinder with Onshape?

If I have a 3D cylindrical extrusion (in Onshape), how can I scoop, carve, or indent a concave/parabolic curve in one of the ends? The yellow surface is the target. Here is the basic shape I'm ...
3
votes
1answer
141 views

Smooth finish on large parts

I would like to print a vase that has a width/length/height footprint of 100x100x200 mm, and the surface finish is of particular interest to me. Ideally, I would like to do a minimum of sanding/XTC-3D ...
3
votes
1answer
37 views

3D printer putting scars on my prints

I just ran a 3D benchy on my Lotmaxx SC-10 3D printer and it came out fantastic. No stringing, melting, the dimensions look good, the bed adhesion is perfect, and it is identical to the 3D model. But ...
3
votes
2answers
163 views

Bad quality at horizontal faces

I'm newbie at this stackexchange and I have a "FlashForge Finder"; lately there are many problems with the horizontal surfaces quality (Bottom and Top at the same time). As some issue guides suggests,...
2
votes
2answers
468 views

What is this white layer on my 3D printer?

I left my printer to print a circular object and when I came back I saw it didn't print anything but left this layer of white on the surface. I can't get it off, I've tried washing it and scraping it ...
2
votes
2answers
142 views

How to remove ABS from PEI Sheet

Recently building a new printer, I went with a Wambam PEX system. When I began printing ABS I found it did not stick very well and eventually purchased a new build plate and a PEI sheet since PEX isn'...
2
votes
2answers
403 views

Weird surface thing

I have a 3D printer at home, the Colido Compact, and for some reason when I 3D print big flat surfaces a really weird thing happens. I'm using some PLA from Colido too I think It almost seems as if ...
1
vote
0answers
36 views

Problem with jitters with Ender 3

Recently I realized that I have been getting jitter-like rough surfaces on round parts of my models from my Ender 3. The jitters happen on the sides of the model, so the jitters would be happening in ...
0
votes
1answer
53 views

How to start a print in the center position after a change in parameters using M92 and M500 G-code

I have a Core XY Custom DIY Printer, but actually I have a problem with the measure in Axis X and Y. When a print a test cube with the measure 20 mm x 20 mm 20 mm, the object printed result with these ...
0
votes
1answer
121 views

Equally spaced surface flaws

I'm having an odd effect in my prints. There is some sort of surface problem that seems to be evenly spaced in z. I tried to tighten my belts, the print speed is 75 mm/s using a 32 bit board, on an ...
0
votes
1answer
72 views

Meshlab creates weird bubbles when using poisson surface reconstruction

my task is to create a watertight surface out of a point-cloud (It's the model of a dam). For this I'm using MeshLab. First thing I did was importing the .ply-file into Meshlab and normalize it. ...
0
votes
0answers
78 views

Zits and blobs caused by Cura. How do I fix this?

I am using a Creality CR-10S Pro and lately I've been having problems with zits and blobs on my surface whenever I do an aesthetic print that has more curves and turns than a functional print would ...