Ender 5 Pro print quality issue
I got my 3D printer from Creality 1 day ago. My dog off the SD card came perfectly, Benchy was also printed almost flawlessly. I used standard Benchy settings on all my prints.
Now I tried making a ...
2
votes
1answer
27 views
Top layer and walls have gaps even with 120 % flow (Cura)
I'm printing with Geeetech A20 printer, PLA.
I've started printing the same test piece while changing the following parameters:
Temperature from 215 °C to 195 °C (lowering by 5 °C on each print)
Flow ...
2
votes
0answers
108 views
Walls are sometimes porous
I have a Tronxy P802E, which works pretty well for me. I currently use Ultimaker Cura 4.1.0. However, I occasionally get a weird problem where the walls in certain parts of certain prints will be ...
1
vote
0answers
40 views
Under-extrusion near the seam
I have an FLSUN QQ-S Pro and I'm trying to print a part consisting only of thin walls with PLA. I'm using Cura 4.8.0, "FLSUS QQ-S" profile. Unfortunately, near the seam there are signs of ...
1
vote
1answer
22 views
CTC i3 Y-axis thin / no filament deposition
I have this CTC i3 printer; when I print square test prints, as it moves along the Y-axis back to zero (front). It extrudes lines but very thin or none at all.
But opposite direction along the Y axis ...
1
vote
0answers
60 views
Consistent blobbing and gaps in print towards right side
Issue:
I'm having a problem with some blobbing and gaps consistently in the same areas. The left edge is always good, the right edge is very bad (especially around the corner) and the front and back ...
1
vote
2answers
178 views
Printer extrudes too little filament at beginning and end of extrusion
I've bought a new type of filament (GreenTEC Pro Natural) for my Anycubic Mega i3 to print some food-safe cookie cutters. Now I have changed the print settings to an extruder temperature of 210 &...
0
votes
0answers
54 views
Under extrusion on one side, but only while printing support material
Trying to print a bracket for pliers, however the support material on the left side always fails by under extruding. The model is left-right symetrical, so the support is the same for both sides. ...
0
votes
1answer
500 views
Creality CR-10 problems with extrusion while printing
I have an extrusion problem with my creality CR 10 3D printer while printing.
I am using a standard 0.4 mm nozzle with a 1.75 mm diameter PLA and I use Cura as my slicer.
This printer ...
0
votes
0answers
23 views
Monoprice Maker (Wanhao Duplicator Clone) Intermittent Underextrusion
I've had a Monoprice Maker (a Wanhao Duplicator clone) for about a year and a half now. I'm printing in an enclosed chamber, and I've had a lot of trouble with it in the past (all sorts of random ...