Questions tagged [warping]

Warping denotes the phenomenon of lifting edges during printing. Warping is a thermal expansion effect due to filament shrinking when cooling down.

Filter by
Sorted by
Tagged with
12
votes
3answers
745 views

Troubleshooting poor adhesion at the edge of the bed

I've been printing for a week now on my new printer and have been getting great results, including great adhesion. However, most of my prints have had a fairly small footprint. Now, I'm stepping up ...
11
votes
5answers
5k views

Prints are now sticking too well to the bed. What to do?

I'm a beginner. I've a Printrbot Play with a heated bed add-on. I'm using it exclusively with PLA. It worked great initially, but then I took the nozzle out and put it back in, and the Z calibration ...
10
votes
11answers
51k views

PLA and bed heating?

I've read different things about PLA and heat-bed. Some say it is not needed, others recommend 60-70°C, but not for the first layers. For larger objects I often have the problem that the object does ...
9
votes
2answers
7k views

Wanhao Duplicator i3 ABS settings

I am looking to others who have successfully printed in ABS using a Wanhao Duplicator i3. I have tried and get a lot of warping and delamination. I tried putting a large box over the printer which ...
8
votes
3answers
1k views

Printing with Polycarbonate keeps warping

I'm trying to print a large piece with polycarbonate but it keeps warping, I'm using a Taz 5 printer and setting 290 C in the extruder and 145 C in the heating bed. Other setting I have are: ...
7
votes
1answer
152 views

My print is warping: how can I ensure that it cools evenly?

My print is warping and I suspect it is because of uneven cooling. How can ensure my print cools evenly? Should I put a fan on the bed? Will no fan and a tall skirt help? Or are my edges curling up ...
6
votes
2answers
5k views

Warping of bottom of print

The bottom of my prints warp/curve upwards, most often at the corners. This is a very slight curve, only about 1-2 mm. I print with a raft all the time. I don't have a heated bed. I print with PLA at ...
5
votes
6answers
8k views

Creality CR-10S Pro 3D printer heated bed turns off after first few layers: normal?

When I run prints on my Creality CR-10S Pro 3D printer (using Ultimaker Cura as slicer), I set the heated bed to around 70 °C for PETG. after the first few layers, the heated bed set point ...
5
votes
5answers
356 views

Great prints then suddenly terrible quality

I've been printing with my Ender 3 for a while now and it's been great. I've had very few problems - depending on my settings, these are my typical first layers: However with no settings or ...
5
votes
3answers
7k views

How to remove a PLA print stuck to a BuildTak sheet

BuildTak is great because the printed plastic really sticks to it, it pretty much solved all the problems I had with prints detaching from the buildplate during printing. However, it does sometimes ...
5
votes
3answers
497 views

Help preventing warping while 3d printing with polypropylene

I am wondering if anyone can help me achieve a good 3d print using polypropylene. I am trying to print custom insoles for shoes and I'm getting some bad warping/lifting (see image). Some details ...
4
votes
3answers
198 views

How to print a 6" wheel in ABS?

I'm using a Flashforge Pro and attempting to print a wheel about 6mm thick to serve as a platform. In other words, the wheel doesn't have to be solid, but spokes won't do the job. I've experimented ...
4
votes
3answers
1k views

Printing shells and pouring filler

I had this idea for bulky parts for just printing the shell (PLA) then pouring in some kind of filler in to make up the bulk/strength. Printing bulk .2mm at a time line by line is slow and subject to ...
4
votes
4answers
3k views

3D prints keep suffering from warping

I have a Prusa i3 made by Geeetech. My 3D prints keep suffering from warping when printing with PLA. Whenever I print something with a base at about 10 cm x 10 cm, at least one corner of the print ...
4
votes
2answers
2k views

Raft warping (Makerbot Replicator+)

Quick thing: Please tell me if I misuse any of the terminology On a replicator+, I have been printing successfully for a while, when suddenly the raft started to warp. I was doing a bunch of models ...
3
votes
3answers
151 views

How to solve ABS deformation at the bottom?

I am printing small mechanical pieces in ABS: 100 ºC bed temperature 70 ºC Room temperature 250 ºC nozzle temperature 0.4 mm nozzle, at 0.15 mm per layer. 100.8 % scale to compensate ABS dimensional ...
3
votes
2answers
6k views

How do you solve PLA corner-curling short of printing really, REALLY slow?

I've been trying a lot of different things to combat corners curling upward in the first few tens of layers after the bottom skin. To be clear, I'm not talking about corners of the first layer printed ...
3
votes
2answers
933 views

Ender-3 Pro - PLA mid-layer warping (layer separation) - salvageable?

I just got into 3D printing with an Ender-3 Pro. The test dog printed great, some custom small/thin objects printed good, and now I tried my first big object. Designed in Tinkercad (link to my (...
3
votes
1answer
80 views

How to get rid of deforming small prints?

When printing a big base on the bed, I got no warping, but once I print small part (3 or less inches wide), there is a bit of warping on my piece as I remove it. It is 2 inches wide by 1 mm ...
2
votes
3answers
496 views

How could I keep the material on the print plate from bending up on a makerbot 2?

I printed a big base for a model, but the corners of the bottom bent up, making the whole base rock when set on a table. Is there a quick fix for a makerbot2 without a heated plate?
2
votes
3answers
140 views

What can I do about a printjob in progress that starts to warp/curl on the edges?

I currently have a print job that is about 50% done, been running for 2 hours with 2 hours remaining. One side is curling/warping pretty bad, and I'm afraid there's no possible way this is going to ...
2
votes
2answers
2k views

Will lowering print temperature help warping?

I realize this issue (warping) has been repeatedly addressed on this site. I've just graduated to high-temp filaments (PC in particular). I don't know much of the physics of this. I'm wondering ...
2
votes
2answers
4k views

PLA print warping on heated bed [duplicate]

I am trying to print the 3 jaw lathe chuck on Thingiverse. This specific piece is the scroll.stl, but it applies on every big piece. The print material is (transparent) PLA, that I print on custom ...
2
votes
1answer
172 views

Warped bed - bulge vs dip?

Theoretically what is better- a warped bed with a dip in the middle, or a bulge in the middle? (I would instinctively think that a dip would be better, since in a perfect world the glass build ...
2
votes
1answer
3k views

PETG warping - adhesion or temperature too high?

Ender3 v2, SIENOC PETG which advises temperature of 230-250 °C on the box. I'm printing on top of cleaned blue tape, using a temperature of 230 °C for the nozzle and 80 °C for the bed. I've had all ...
2
votes
3answers
604 views

How to prevent bend (or warping) with M3D printer?

Hello is there a way to prevent bend on print with M3D printer?
1
vote
2answers
631 views

Does moisture cause warping?

I'm printing flat objects (like rectangular) with PLA on a glass bed and 70 celcius degrees (also tried 75 celcius too, 65 celcius and lower ends with adhesion problem in general). Also I use brims ...
1
vote
2answers
803 views

TPE warping problems

I'm attempting to print some flexible TPE filament. But I failed to imagine TPE was this difficult to print. Specs of the shop-brand filament: Red 1.75 mm TPE (+-0.05 mm). Hardness: 45D. ...
1
vote
1answer
85 views

How to set multiple draft shields in Prusaslicer?

Draft shields helped me a lot to get some usable prints out of ABS on a non-enclosed printer with a small printing bed, but I noticed that the shield cracks (it is affected by the issue that would ...
1
vote
1answer
175 views

Problem printing bigger models in the Ender 5

In all the bigger prints I print on my Ender 5 with PETG I have problems with warping and raft detachment during printing. I have a glass bed and I'm using Ultimaker Cura 4.6.1 standard printing ...
1
vote
0answers
50 views

PLA Warps despite every effort to prevent it

I am using a Creality Ender 5 with a tempered glass bed. I could say that I am a seasoned 3D printing hobbyist but I am really out of ideas in this case. Currently I am using a grey colored PLA that ...
1
vote
0answers
86 views

Why does printing outer walls last cause corner curling?

In an old question I just self-answered, I had ongoing problems with corner curling that went away due to my switching to using Cura's Outer Before Inner Walls (...
0
votes
1answer
37 views

Can parts that have warped (after being printed) be un-warped?

I have an on-going project to build a large lampshade in the shape of a geodesic dome. It's made of 3D printed frames that will be covered with rice paper. I printed the parts in PLA over a month or ...