"Seams" in first layer

Normally, such patterns are caused by too close printing to the bed (nozzle to bed distance too small), but considering the not fully flattened out extrusion lines (on glass I get a mirror shine fully ...
user avatar
  • 31k
1 vote
Accepted

Any possible issues with adding heat/cool down cycle in the end of print (PLA)

Heating PLA even to 60°C will make it pliable and may affect dimensional accuracy; 100°C is likely to make that severe. Being stuck to the bed and thus constrained by it might help some, but I think ...