1 vote
0 answers
108 views

Bioprinter does not extrude Anet A8 Marlin

I have a modified Anet A8 that is supposed to print hydrogels (paper : Ultra-Low-Cost 3D Bioprinting, Kahl M et al. 2019). For this to work, we do not need any temperature-related settings, however, I ...
Andris Gyori's user avatar
4 votes
1 answer
4k views

Massive over extrusion after changing firmware

I have an Anet A8 printer (no modifications) and first printed a calibration cube. It came out okayish, within expectations. Afterwards I flashed the firmware to Marlin 1.1.9 and since then have very ...
Till B's user avatar
  • 313
1 vote
1 answer
755 views

Stuck getting ANet A8 Printer to build layers [duplicate]

I have excitedly decided to get my feet wet in the 3D printing world, and being that budget is fairly small got myself an ANet A8 3D printer. I have it all assembled and am able to 'print' however I ...
user1829564's user avatar
7 votes
3 answers
1k views

Anet A8 bad/inconsistent extrusion after changing nozzle

I just changed my nozzle on my Anet A8 after it was fully used up. When I started printing with my new 0.4 mm nozzle (same as before) my extrusion was VERY bad and inconsistent, even so bad I ...
HugoG's user avatar
  • 71
2 votes
1 answer
2k views

Cooling time query ABS

I printed Thingiverse "Benchy" at the default Anet settings for ABS, hot end and bed, as a first test. The result was fair but needs a bit of tweeking. The model was removed from the "hot bed" and set ...
Plodmore's user avatar
  • 367
6 votes
1 answer
883 views

Filament not extruding

I've recently bought an Anet A8, and haven't been getting good prints with it. I noticed there was filament leaking from the top of the hot end and pooling, eventually dripping over onto my prints. I ...
Gentatsu's user avatar
  • 161