1
$\begingroup$

So I have printed multiple benchies with various slicer settings. I have also made sure my bed is leveled well.

But no matter what I do, I get these over extrusion whenever my nozzle is moving in diagonals (left-right). It's always this same angle where it goes wrong.

Has anyone else who has faced this and has figured out know what the issue can be? I'm new to 3D printing so the help would be very much appreciated.

Picture of sample extrusion problem

$\endgroup$
1
  • 1
    $\begingroup$ Please tell us what printer, what slicer, and what firmware you are using. Your slicer settings will help as well. $\endgroup$
    – Davo
    Jun 10 '21 at 15:47
2
$\begingroup$

The issue was that the X-axis belt was super loose, figured it after someone pointed it out on Reddit:

swordfish45

You have an extremely loose x belt. That's the root cause of all your problems I can see in these pics.

$\endgroup$
1
  • 1
    $\begingroup$ Thanks for answering your own question! Please accept the answer after 48 hours after posting! Thanks. $\endgroup$
    – 0scar
    Jun 11 '21 at 5:55

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.