Search Results
Search type | Search syntax |
---|---|
Tags | [tag] |
Exact | "words here" |
Author |
user:1234 user:me (yours) |
Score |
score:3 (3+) score:0 (none) |
Answers |
answers:3 (3+) answers:0 (none) isaccepted:yes hasaccepted:no inquestion:1234 |
Views | views:250 |
Code | code:"if (foo != bar)" |
Sections |
title:apples body:"apples oranges" |
URL | url:"*.example.com" |
Saves | in:saves |
Status |
closed:yes duplicate:no migrated:no wiki:no |
Types |
is:question is:answer |
Exclude |
-[tag] -apples |
For more details on advanced search visit our help page |
Questions about part-to-platform or layer-to-layer adhesion while 3D printing.
1
vote
Accepted
Are all glue sticks PVA-based? How to find out?
water; a defoamer; a bactericide; an oil; polyvinylpyrrolidone; a plurality of polyurethane dispersions; dipropylene glycol n-butyl ether; sodium stearate; casein; sodium hydroxide; and at least one adhesion …
0
votes
Polypropylene Bed Adhesion
The other issue with adhesion is the greater the difference between the extruder temperature and the bed the poorer adhesion. There are other things can help with this. … A slower extrusion speed allows the extrusion to cool more before getting as long of a length to for the contraction force; thus improving adhesion. …
0
votes
Irregular adhesion on Creality glass bed
I haven't seen lifts that aren't on the edge of the print, such as warping, or the entire printed surface lifts. When I get something like in your photograph, it's because the print surface isn't fla …
4
votes
Accepted
Has anyone applied four 200 x 200 mm PEI sheets to a 400 x 400 mm bed?
Aligning build surfaces isn't the main issue with 1 mm thick surfaces when aligning four 200 x 200 mm surfaces to make one 400 x 400 surface. The main issue is slight bucking at the seams from therma …
0
votes
CR-6 SE glass build plate - no lifting possible
Sounds like the bed came with a coating on it. If you can't find out what the coating is, but believe you already removed it, you could try glue sticks or hair spray. You can also find glue sticks s …
1
vote
Print not sticking to bed
Your temperatures look pretty good. You could try raising both bed temperatures by 5°C.
You could try Elmer's glue stick or hair spray.
Make sure your Z height is still OK as well as your bed being l …
3
votes
How to remove ABS from PEI Sheet
Heat up your bed to the print temperature; maybe even as hot as 100 °C. This will soften the ABS and make it easier to scrape off. It will distort a print to remove it this way, but is good for clea …
1
vote
What's causing my PLA prints to lift like this?
Use a higher extrusion temperature for the first layer to promote adhesion. (Differences in PLA composition could cause these temperatures to vary.) … Sometimes it helps to have an bed temperature for the 1st layer as high as 75 °C to promote adhesion. …
1
vote
What techniques are needed to minimise layer separation after filament change?
Most of your settings will not change with changing filament, if the new filament is the same material and OEM as the old. The main settings to check after changing the filament are the initial z-hei …
2
votes
My Hatchbox PLA filament only allows me to use rafts
This is a first layer adhesion issue.
Your bed may not be clean, or the bed may have had an adhesion layer you cleaned off.
Your nozzle may be too high on the first layer. … Glue sticks can help adhesion. Glue sticks usually don't post the composition on the packaging, but Elmer's glue sticks work. …
0
votes
Problem printing bigger models in the Ender 5
As reported by others, I get much less warping with PETG than with ABS or even PLA, and deal with too much adhesion with PETG rather than too little. …