Linked Questions
14 questions linked to/from What are ways to avoid heat creep?
4
votes
4
answers
4k
views
Ender 3 V2 Extruder getting hot
I'm still fairly new to 3D printing; got my Ender 3 V2 for Christmas last year. Recently the tension arm in the stock extruder snapped, so I bought and installed an all-aluminum replacement. My first ...
2
votes
3
answers
3k
views
Printer has stopped extruding
I have been printing toy cars for about a month now and my Ender 3 has stopped extruding plastic even when I insert filament, it has been about a day since it stopped working. Is there any tips for ...
4
votes
4
answers
2k
views
Prusa MK3S not extruding during printing but extruder working
I didn't have any printer-related problem for the past 6 months, but now all of a sudden my Prusa MK3S stopped extruding during printing.
This is very strange as I can easily load\unload filament and ...
3
votes
2
answers
3k
views
Extruder stops printing before finishing first layer (Ender 3 v2 w/BIQU H2)
Let me preface this with me being quite a newbie to 3D printing, however, I am an engineer and coder, so tinkering with stuff like this is quite the norm for me. Don't be afraid to be too technical, ...
3
votes
3
answers
2k
views
Filament end expanding and seizing
This is a continuation of this question where comments and answers were extremely helpful in diagnosing the issue, which I am still unable to solve.
I determined I have the problem shown in figure 3 ...
2
votes
2
answers
2k
views
PLA Jamming- is the heat break too hot or too cold?
I’m getting nothing but jams with a new BCN3D Sigma R19 printer, printing PLA at 195 °C, two brands (BCN’s own brand and Monoprice orange). 6.5 mm retraction, as used in BCN’s PLA profile. Using their ...
3
votes
1
answer
975
views
How is heat creep characterized?
I have a Delta printer with Bowden extruder and all-metal hotend. When I start printing, the hotend gets often jammed. It seems to be independent of the print I am currently doing. Retraction does not ...
2
votes
1
answer
1k
views
Ender 3 v2 - Filament clog before nozzle
The filament "swells" up to the inner diameter of the feeding pipe, from the nozzle to about the end of the heat-sink. This happens after a few hours of printing. It happened using a new ...
1
vote
3
answers
919
views
Filament jam on the tube entrance
I have a problem in regards to filament jam, however I don't think that my case is any related to the extruder nozzle.
After 30 to 40 minutes printing my filament bends and get stuck on the tube ...
2
votes
1
answer
1k
views
Filament getting stuck/nozzle is clogged
For some reason on my Raise 3D N2 plus with a Bondtech-Extruder I am sometimes seeing filament jams and sometimes it prints without any issues. I am using PLA at 215 °C.
When the filament is jammed I ...
2
votes
1
answer
1k
views
Ender 3 v2 printing problem [closed]
Last week, my printer worked really well, but after a print it started having some printing problems. The printer stops extruding mid-print or under extrudes.
After this happened, I
leveled the bed ...
3
votes
2
answers
702
views
Material to use inside ultrasonic cleaner
I am trying to create a couple of holders for my ultrasonic cleaners. They are supposed to be used for parts that don't fit in the holder that came with the cleaners. I was wondering what material is ...
1
vote
3
answers
652
views
Air printing/jamming midway through raft creation
For a school project, my teacher gave me a brand new Longer 3D printer to create parts with. After one good job, the printer cannot get past the raft creation without air printing. The thickness of ...
2
votes
3
answers
265
views
Extrusion issues on medium speeds (while accelerating?)
I've recently changed my Ender3's hotend to E3D v6 clone with Titan direct extruder, so I can print faster than on stock. But when I increased the speed up to 70 mm/s for walls and 80 mm/s for infill (...